Epoxy Anti-corrosive Finish



This product is a two-component product based on epoxy resin, added with polyamide curing agent.It has the following resistance characteristics:

  • Strong Adhesion

  • Good Flexibility

  • Wear Resistance

  • Water Resistance

  • Oil Resistance

  • Chemical Resistance




Epoxy Anti-corrosive Finish Basic Technical Datasheet



Color

Customized

Gloss

Glossy

Density

~1.25Kg/L (after mixing)

Hardness

Epoxy paint curing agent

Solid Volume

(48±2 )%

Standard Film thickness

80um dry film thickness  (about 160um wet film thickness)

Theoretical spreading rate

5m²/Kg (60um dry film thickness)

Full Cure

(23±2℃ )7d

Flash Point

27℃

01


Epoxy Anti-corrosive Finish Product Packaging

Packaging:

part A:20kg in a 20-liter iron bucket.

part B:5kg in a 6-liter iron bucket.

Shelf Life:

12 months If exceeding shelf life, the products shall be tested before using.




Epoxy Anti-corrosive Finish Applicable Environment


1 2 3 4

Separation Equipment

Offshore facilities

Bridges

Reactor

5 6造纸 7电厂设备 8脱硝反应外壳
Pipeline Paper Mill Power Plant De-NOₓ Equipment



Epoxy Anti-corrosive Finish Compatibility




Product Thickness

Primer:

Epoxy Iron Oxide Red Primer or

Epoxy Zinc Phosphate Primer


2*50 µm (dry film thickness)


Paint:

Epoxy Anti-corrosive Finish


2*40 µm (dry film thickness)



Epoxy Anti-corrosive Finish Finished Projects


9 10 11

 


Epoxy Anti-corrosive Finish Production Process


4-1 4-2 4-3



Epoxy Anti-corrosive Finish Instructions For Use



Substrate Treatment:

The surface to be coated shall be clean, dry and free from contaminations. Also, the surface shall be evaluated and treated according to ISO8504 standard.

Bare steel: sandblasting to reach Sa2.5(IOS8501-1:2007). For the non-soaking site, acceptable for power tool grinding, at least reach St2(IOS8501-1:2007).

Instructions for Use:

  • Mixing:

Use the power mixer to mix the main paint evenly, and then as you stir it, you add the hardener until you get to mix well. Generally, if the temperature is below 10℃, it needs 30 min induction time; If the temperature is over 10℃, it needs 15 min induction time.

  • Mixing Ratio:

Part A: Part B= 20:5 (by weight)

  • Thinner:

Epoxy paint thinner

  • Airless spray:

Nozzle tip: 0.021~0.025 inches

Spray pressure: 15~18Mpa

Thinner ratio: 0~15% (by weight of paint)

  • Brush、Roller:

Recommended Must achieve required thickness





Epoxy Anti-corrosive Finish Company Introduction




8-1
6-1 6-2 6-3 6-4



Epoxy Anti-corrosive Finish Exhibitions



7-1 7-2 7-3
7-4 7-5 7-6








Previous: 
Next: 
Apply Our Best Quotation
Apply Our Best Quotation
If you have any questions about our products, reach out to YMS Paint customer service team.
    inquiry@jsbj88.com
   +86-18015818726
  +86-519-85506198

Products

Application

Quick Links

© COPYRIGHT 2024 CHANGZHOU YMS NEW MATERIALS TECHNOLOGY CO., LTD. ALL RIGHTS RESERVED.