YMS
7-15days
200kg
10T/day
Shanghai,Qingdao,Guangzhou,Ningbo etc
Customized(Iron red if used as primer)
Flat
~1.45Kg/L(after mixing)
Use the power mixer to mix the main paint evenly, and then as you stir it, you add the hardener until you get to mix well. Generally, if the temperature is below 10℃, it needs 30 min induction time; If the temperature is over 10℃, it needs 15 min induction time
Part A: Part B= 20:5 (by weight)
3.68m²/Kg (150um dry film thickness)
| Availability: | |
|---|---|
High-build Epoxy High Solid Volume Paint
This product is a two-component high solid volume thick paste coating based on epoxy resin and amine curing agent.It has the following resistance characteristics:
|
|
|
| ||
High-build Epoxy High Solid Volume Paint Video
Color | Customized(Iron red if used as primer) |
Gloss | Flat |
Density | ~1.45Kg/L(after mixing) |
Hardness | Epoxy paint curing agent |
Solid Volume | (80±2 )% |
Standard Film thickness | 150um dry film thickness (about 190um wet film thickness) |
Theoretical spreading rate | 3.68m²/Kg (150um dry film thickness) |
Full Cure | (23±2℃ )7d |
Flash Point | 35℃ |
![]() | High-build Epoxy High Solid Volume Paint Product PackagingPackaging: Part A 20kg in a 20-liter iron bucket. Part B 5kg in a 6-liter iron bucket. Shelf Life: 12 months If exceeding shelf life, the products shall be tested before using. |
![]() | ![]() | ![]() | ![]() |
Offshore Platform | Pharmaceutical Workshop | Reactor | Crude Oil Storage Tank |
![]() | ![]() | ![]() | ![]() |
| Pipeline | Wharf Facilities | Desulfurization Tower | Distillation Column |
| Product | Thickness | |
Primer: | Epoxy Zinc Rich Primer | 2*40 µm (dry film thickness) |
Paint: | Epoxy Mica Iron Oxide Intermediate Paint | 2*40 µm (dry film thickness) |
Topcoat: | Epoxy High Solid Volume Thick Paste Paint | 2*75 µm (dry film thickness) |
![]() | ![]() | ![]() |
![]() | ![]() | ![]() |
Substrate Treatment:
All surfaces to be coated shall be clean and dry. The surface shall be evaluated and treated according to ISO8504 standard.
For bare steel, it shall be sandblasted to reach Sa2.5(iso8501-1:2007) standard. Depending on the environment of the non-immersed part, grinding with power tools is acceptable but shall at least reach St2(iso8501-1:2007) standard.
For shop primed steel, the shop primer shall be clean, dry and approved.
For surface painted coatings, this product can apply only to clean, dry and good compatible primer.
Instructions for Use:
Mixing:
Use the power mixer to mix the main paint evenly, and then as you stir it, you add the hardener until you get to mix well. Generally, if the temperature is below 10℃, it needs 30 min induction time; If the temperature is over 10℃, it needs 15 min induction time.
Mixing Ratio:
Part A: Part B= 20:5 (by weight)
Thinner
Epoxy paint thinner
Airless spray
Nozzle tip: 0.017~0.025 inches
Spray pressure: 15~18Mpa
Thinner ratio: 0~15% (by weight of paint)
Brush、Roller
Recommended
Must achieve required thickness
![]() | |||
![]() | ![]() | ![]() | ![]() |
![]() | ![]() | ![]() |
![]() | ![]() | ![]() |
High-build Epoxy High Solid Volume Paint
This product is a two-component high solid volume thick paste coating based on epoxy resin and amine curing agent.It has the following resistance characteristics:
|
|
|
| ||
High-build Epoxy High Solid Volume Paint Video
Color | Customized(Iron red if used as primer) |
Gloss | Flat |
Density | ~1.45Kg/L(after mixing) |
Hardness | Epoxy paint curing agent |
Solid Volume | (80±2 )% |
Standard Film thickness | 150um dry film thickness (about 190um wet film thickness) |
Theoretical spreading rate | 3.68m²/Kg (150um dry film thickness) |
Full Cure | (23±2℃ )7d |
Flash Point | 35℃ |
![]() | High-build Epoxy High Solid Volume Paint Product PackagingPackaging: Part A 20kg in a 20-liter iron bucket. Part B 5kg in a 6-liter iron bucket. Shelf Life: 12 months If exceeding shelf life, the products shall be tested before using. |
![]() | ![]() | ![]() | ![]() |
Offshore Platform | Pharmaceutical Workshop | Reactor | Crude Oil Storage Tank |
![]() | ![]() | ![]() | ![]() |
| Pipeline | Wharf Facilities | Desulfurization Tower | Distillation Column |
| Product | Thickness | |
Primer: | Epoxy Zinc Rich Primer | 2*40 µm (dry film thickness) |
Paint: | Epoxy Mica Iron Oxide Intermediate Paint | 2*40 µm (dry film thickness) |
Topcoat: | Epoxy High Solid Volume Thick Paste Paint | 2*75 µm (dry film thickness) |
![]() | ![]() | ![]() |
![]() | ![]() | ![]() |
Substrate Treatment:
All surfaces to be coated shall be clean and dry. The surface shall be evaluated and treated according to ISO8504 standard.
For bare steel, it shall be sandblasted to reach Sa2.5(iso8501-1:2007) standard. Depending on the environment of the non-immersed part, grinding with power tools is acceptable but shall at least reach St2(iso8501-1:2007) standard.
For shop primed steel, the shop primer shall be clean, dry and approved.
For surface painted coatings, this product can apply only to clean, dry and good compatible primer.
Instructions for Use:
Mixing:
Use the power mixer to mix the main paint evenly, and then as you stir it, you add the hardener until you get to mix well. Generally, if the temperature is below 10℃, it needs 30 min induction time; If the temperature is over 10℃, it needs 15 min induction time.
Mixing Ratio:
Part A: Part B= 20:5 (by weight)
Thinner
Epoxy paint thinner
Airless spray
Nozzle tip: 0.017~0.025 inches
Spray pressure: 15~18Mpa
Thinner ratio: 0~15% (by weight of paint)
Brush、Roller
Recommended
Must achieve required thickness
![]() | |||
![]() | ![]() | ![]() | ![]() |
![]() | ![]() | ![]() |
![]() | ![]() | ![]() |