Polyurethane Mica Iron Oxide Intermediate Paint
High-Build Shield for Steel Structures
A two-component intermediate paint composed of hydroxyl epoxy resin containing carboxyl group, anti-rust pigments, lamellar mica iron oxide, fillers, auxiliaries and PAPI polyisocyanate curing agent. The plate-like pigment builds a tortuous barrier for thick-film shielding, rust resistance, fast drying and oil resistance — with excellent intercoat adhesion between primer and finish.
Technical Parameters
Polyurethane Mica Iron Oxide Intermediate Paint — key figures
| Color | Gray, reddish-brown |
|---|---|
| Gloss | Flat / glossy (semi-gloss grade available on request) |
| Composition | Two-component intermediate paint: hydroxyl epoxy resin containing carboxyl group, anti-rust pigments, lamellar mica iron oxide, fillers, auxiliaries and PAPI polyisocyanate curing agent |
| Mixing ratio | Part A : Part B = 20 : 4 by weight |
| Density | ~1.55 kg/L after mixing |
| Solid volume | (55 ± 2)% |
| Standard film thickness | 100 µm dry film thickness (about 180 µm wet film thickness) |
| Theoretical spreading rate | 3.55 m²/kg at 100 µm DFT (4.2 m²/kg at 80 µm DFT on some datasheets) |
| Hardness | Polyurethane curing-agent system |
| Flash point | Part A: 32°C · Part B: 27°C |
| Drying schedule (40 µm) | To touch: 4 h @10°C / 2 h @20°C / 1 h @30°C · To handle: 24 h / 12 h / 6 h · Min. recoat: 16 h / 8 h / 4 h · Pot life: 4 h / 2 h / 1 h |
| Mixing | Power-mix Part A evenly, then add Part B and stir until fully homogeneous |
| Thinner | Polyurethane thinner |
| Airless spray | Nozzle tip 0.017–0.023 inches · spray pressure 15–18 MPa · thinner 5–15% by weight of paint |
| Brush / roller | Recommended for small areas only — must achieve the required film thickness |
| Application conditions | Substrate temperature at least 3°C above dew point; relative humidity below 85%; measure close to the substrate |
| Surface treatment | ISO 8504 evaluation; bare steel sandblasted to Sa2.5 (ISO 8501-1:2007); power-tool grinding at least St2 outside immersion service; shop primer clean, dry and approved |
| Classic coating system | Polyurethane primer 2 × 40 µm DFT · Mica iron oxide intermediate 2 × 50 µm DFT · Polyurethane finish 2 × 40 µm DFT |
| Packaging | Part A: 20 kg in a 20-litre iron bucket · Part B: 4 kg in a 5-litre iron bucket |
| Shelf life | 12 months in a shady, dry, ventilated warehouse; test before use if exceeded |
| Certificates | CE, ISO 9001, ISO 14001, OHSAS 18001, RoHS, SASO, SGS and SRC available on request |
* Drying, recoat and pot-life data are reference values; actual performance depends on substrate temperature, dry film thickness and ventilation. Refer to the MSDS before use. Full TDS, MSDS and test reports are available on request.
Packaging & Supply
Factory-direct two-component sets from the YMS / JIANBANG plant
- 20 kg + 4 kg Component SetsPart A: 20 kg in a 20-litre iron bucket. Part B: 4 kg in a 5-litre iron bucket. Supplied at a 20:4 weight mixing ratio for consistent batch-to-batch build.
- MOQ 200 kg · Fast DispatchMinimum order 200 kg per product, with 7–15 day delivery and 10 T/day production capacity. Shipped from Shanghai, Qingdao, Guangzhou, Ningbo and other ports.
- System & Color MatchingGray and reddish-brown standard, flat or glossy. Our technical team matches primer, intermediate and finish to your steel structure and exposure environment.
- 12-Month Shelf LifeStore in a shady, dry, ventilated warehouse. Test before use if the shelf life is exceeded. TDS, MSDS, CE/RoHS/ISO documents and test reports ship with every order.
Core Functions
What this high-build intermediate layer does for the coating system
100 µm DFT in One Pass
A high-solid (55 ± 2%) intermediate coat lays down about 100 µm dry film — 180 µm wet — so the classic system reaches its build with 2 × 50 µm intermediate coats.
Mica Iron Oxide Shields Steel
Plate-like mica iron oxide flakes overlap into a tortuous path that slows moisture and oxygen reaching the steel surface.
Recoat in 4–16 Hours
At 40 µm DFT: touch dry in 1–4 h, handle dry in 6–24 h and ready for recoat in 4–16 h across 10–30°C.
Built for Industrial Environments
The cured polyurethane network resists oil and common industrial media, making it a dependable middle layer in demanding service.
The Bridge Between Primer & Finish
Engineered as the system layer: excellent contact and adhesion with compatible polyurethane primers and topcoats.
From Cranes to Wind Towers
Specified for port cranes, bridges, transmission towers, workshops, guardrails, wind turbine towers, canopies and storage racks.
Applications
Where Polyurethane Mica Iron Oxide Intermediate Paint goes on
Thick-film mica iron oxide shielding on harbor gantry cranes and terminal steelwork exposed to salt-laden atmospheres.
Girders and cross beams stay protected through traffic vibration, temperature cycles and year-round weather.
Reddish-brown intermediate build on tall steel towers, paired with a weather-resistant polyurethane finish.
Lattice steel structures gain a durable barrier layer before the topcoat goes on.
Columns, beams and racking protected against corrosion and daily handling wear inside busy facilities.
Roadside steel and canopy frameworks insulated from moisture with a high-build intermediate coat.
How to Use · 4-Step Application Procedure
From Sa2.5 steel preparation to a complete PU coating system
Note: surface preparation follows ISO 8504 / ISO 8501-1 and the YMS / JIANBANG datasheet. This product is flammable — keep away from flame, prohibit smoking, ventilate the work area and wear PPE. Dispose of used barrels responsibly.
See It In Action
Application and quality-control moments on real facade projects
On-site spray application builds the specified 100 µm dry film on prepared steel facade members.
Coating thickness is checked on real facade panels before the polyurethane finish is applied.
Finished facade steelwork is inspected for uniform build, surface quality and system continuity.
Why Choose YMS Paint / JIANBANG Coatings
Protective coating systems with documents, capacity and export experience
One Anticorrosion Platform, Four System Layers
Build the full primer → intermediate → finish stack
Polyurethane Mica Iron Oxide Intermediate Paint
This product — lamellar high-build bridge coat, 100 µm DFT, A:B 20:4, fast drying.
Epoxy Micaceous Iron Oxide Intermediate
High-build epoxy alternative for severe corrosion environments where maximum barrier performance is required.
Polyurethane Primer
Red-oxide PU primer applied at 2 × 40 µm DFT as the base of the classic three-coat system.
Acrylic Polyurethane Topcoat
Weather-resistant decorative finish applied at 2 × 40 µm DFT for color and gloss retention.
Frequently Asked Questions
What is Polyurethane Mica Iron Oxide Intermediate Paint?
A two-component intermediate paint composed of hydroxyl epoxy resin containing carboxyl group, anti-rust pigments, lamellar mica iron oxide, fillers, auxiliaries and PAPI polyisocyanate curing agent. It builds a thick, shielding layer between primer and finish.
Why use mica iron oxide in the middle coat?
The plate-like mica iron oxide flakes overlap to create a tortuous barrier that slows moisture and oxygen penetration. Combined with high solids and thick-film build, this delivers strong shielding and rust resistance.
What film thickness and coverage should I expect?
Standard dry film thickness is 100 µm (about 180 µm wet), with a theoretical spreading rate of 3.55 m²/kg at 100 µm DFT. Some datasheets quote 4.2 m²/kg at 80 µm DFT. The classic system uses 2 × 50 µm for the intermediate coat.
How is the coating mixed and applied?
Power-mix Part A, then add Part B at 20:4 by weight and mix thoroughly. Use polyurethane thinner at 5–15% for airless spray with a 0.017–0.023 in tip at 15–18 MPa. Brush and roller are recommended for small areas only.
What are the drying and recoat times?
At 40 µm DFT: touch dry 4 h / 2 h / 1 h, handle dry 24 h / 12 h / 6 h, minimum recoat 16 h / 8 h / 4 h, pot life 4 h / 2 h / 1 h at substrate temperatures of 10 / 20 / 30°C.
What surface preparation is required?
Clean and dry surfaces per ISO 8504. Bare steel should be blasted to Sa2.5 (ISO 8501-1:2007); power-tool cleaning to at least St2 is acceptable outside immersion service. Keep the substrate 3°C above dew point and RH below 85%.
What is the classic coating system?
Polyurethane primer 2 × 40 µm DFT, polyurethane mica iron oxide intermediate 2 × 50 µm DFT, and polyurethane finish 2 × 40 µm DFT. Contact our team for a system matched to your structure.
How is it packed and how long does it last?
Part A: 20 kg in a 20-litre iron bucket; Part B: 4 kg in a 5-litre iron bucket. Shelf life is 12 months in shady, dry, ventilated storage; test before use if exceeded. MOQ is 200 kg with 7–15 day delivery.
Get a Sample & an Anticorrosion System for Your Steel Structure
Tell us the substrate, exposure environment, target film thickness and topcoat — our engineers reply within 24 hours with a matched system, coverage estimate and quotation.
Or reach us directly: WhatsApp +86-18015818726 · ymsrecord@jsbj88.com · reply within 24 hours.
WhatsApp Us · +86-18015818726 Email: ymsrecord@jsbj88.com