YMS
7-15days
200kg
10T/day
Shanghai,Qingdao,Guangzhou,Ningbo etc
Orange
Matt, Flat
~1.4Kg/L (after mixing)
38℃
(45±2 )%
Use the power mixer to mix the main paint evenly, and then as you stir it, you add the hardener until you get to mix well.
4m²/Kg (80um dry film thickness)
| Availability: | |
|---|---|
Epoxy Red Lead Anti-rust Primer
This two-component product is composed of epoxy resin, red lead, anti-rust pigment, amine curing agent, auxiliaries, etc.It has the following resistance characteristics:
|
|
| |
Color | Orange |
Gloss | Matte, Flat |
Density | ~1.4Kg/L (after mixing) |
Solid Volume | (45±2 )% |
Standard Film thickness | 80um dry film thickness (about 178um wet film thickness) |
Theoretical spreading rate | 4m²/Kg (80um dry film thickness) |
Flash Point | 38℃ |
![]() | Epoxy Red Lead Anti-rust Primer Product PackagingPackaging: Part A 25KG are packaged in a 20L iron drum. Part B 3KG are packaged in a 3.7L iron drum. Shelf Life: 12 months If exceeding shelf life, the products shall be tested before using. |
![]() | ![]() | ![]() | ![]() |
| Pipeline | Sedimentation tank | Bridge | Workshop beams and columns |
![]() | ![]() | ![]() | ![]() |
| Storage tank | Ship hull bottom | Reaction kettle | Offshore wind turbine tower |
| Product | Thickness | |
Primer: | Epoxy Red Lead Anti-rust Primer | 2*40 µm (dry film thickness) |
| Topcoat: | Epoxy Mica Iron Oxide Intermediate Paint | 2*35 µm (dry film thickness) |
| Topcoat: | Epoxy Finish Paint | 2*40 µm (dry film thickness) |
![]() | ![]() | ![]() |
![]() | ![]() | ![]() |
Substrate Treatment:
The surface to be coated shall be clean, dry and free from contaminations. Also, the surface shall be evaluated and treated according to ISO8504 standard.
Bare steel: sandblasting to reach Sa2.5(IOS8501-1:2007). For the non-soaking site, acceptable for power tool grinding, at least reach St2(IOS8501-1:2007).
Painted surface: only apply to clean, dry and intact compatible primer.
Instructions for Use:
Mixing:
Use the power mixer to mix the main paint evenly, and then as you stir it, you add the hardener until you get to mix well.
Thinner:
Exclusive epoxy paint thinner
Airless spray:
Nozzle tip: 0.017~0.023inches
Spray pressure: 15~18Mpa
Thinner ratio: 5~15% (by weight of paint)
Brush, Roller:
Recommended Must achieve required thickness
![]() | |||
![]() | ![]() | ![]() | ![]() |
![]() | ![]() | ![]() |
![]() | ![]() | ![]() |
Epoxy Red Lead Anti-rust Primer
This two-component product is composed of epoxy resin, red lead, anti-rust pigment, amine curing agent, auxiliaries, etc.It has the following resistance characteristics:
|
|
| |
Color | Orange |
Gloss | Matte, Flat |
Density | ~1.4Kg/L (after mixing) |
Solid Volume | (45±2 )% |
Standard Film thickness | 80um dry film thickness (about 178um wet film thickness) |
Theoretical spreading rate | 4m²/Kg (80um dry film thickness) |
Flash Point | 38℃ |
![]() | Epoxy Red Lead Anti-rust Primer Product PackagingPackaging: Part A 25KG are packaged in a 20L iron drum. Part B 3KG are packaged in a 3.7L iron drum. Shelf Life: 12 months If exceeding shelf life, the products shall be tested before using. |
![]() | ![]() | ![]() | ![]() |
| Pipeline | Sedimentation tank | Bridge | Workshop beams and columns |
![]() | ![]() | ![]() | ![]() |
| Storage tank | Ship hull bottom | Reaction kettle | Offshore wind turbine tower |
| Product | Thickness | |
Primer: | Epoxy Red Lead Anti-rust Primer | 2*40 µm (dry film thickness) |
| Topcoat: | Epoxy Mica Iron Oxide Intermediate Paint | 2*35 µm (dry film thickness) |
| Topcoat: | Epoxy Finish Paint | 2*40 µm (dry film thickness) |
![]() | ![]() | ![]() |
![]() | ![]() | ![]() |
Substrate Treatment:
The surface to be coated shall be clean, dry and free from contaminations. Also, the surface shall be evaluated and treated according to ISO8504 standard.
Bare steel: sandblasting to reach Sa2.5(IOS8501-1:2007). For the non-soaking site, acceptable for power tool grinding, at least reach St2(IOS8501-1:2007).
Painted surface: only apply to clean, dry and intact compatible primer.
Instructions for Use:
Mixing:
Use the power mixer to mix the main paint evenly, and then as you stir it, you add the hardener until you get to mix well.
Thinner:
Exclusive epoxy paint thinner
Airless spray:
Nozzle tip: 0.017~0.023inches
Spray pressure: 15~18Mpa
Thinner ratio: 5~15% (by weight of paint)
Brush, Roller:
Recommended Must achieve required thickness
![]() | |||
![]() | ![]() | ![]() | ![]() |
![]() | ![]() | ![]() |
![]() | ![]() | ![]() |