You are here: Home » Products » Epoxy Paint » Red Oxide Primer » H53-5 Epoxy Red Oxide Primer | Anti-Corrosion Metal Coating for Industrial & Automotive Use

H53-5 Epoxy Red Oxide Primer | Anti-Corrosion Metal Coating for Industrial & Automotive Use

  • H53-5

  • YMS

  • Iron oxide red, semi-gloss

  • ~2.38kg/l

  • Part A: 24℃ Part B: 27℃

  • 55 ± 3%

  • 50cm

  • Mix part A and part B as 25:3 by weight. Slowly add part B into part A and ensure mixed completely.

  • 0.27

Availability:
facebook sharing button
twitter sharing button
line sharing button
wechat sharing button
linkedin sharing button
pinterest sharing button
whatsapp sharing button
sharethis sharing button



H53-5 Epoxy Red Oxide Primer



This two-component primer is mainly prepared with epoxy resin, antirust pigment and curing agent. This product features:


  • Rust resistance

  • Quick drying

  • Water resistance

  • Chemical resistance

  • Excellent adhesion

  • Mechanical properties



H53-5 Epoxy Red Oxide Primer Video




H53-5 Epoxy Red Oxide Primer

Basic Technical Datasheet


Color

Iron oxide red, semi-gloss

Density, kg/L

~2.38

Flash point, ℃

Part A: 24   Part B: 27

Volume solid, %

55 ± 3

Impact resistance, cm

50

Pot life, h

5~6

Theoretical spreading rate, kg/m2 @ 80 µm dry film

0.27

Theoretical spreading rate, kg/m2 @ 80 µm dry film

0.3

VOC, g/L

420
环氧氧化红漆




H53-5 Epoxy Red Oxide Primer Product Packaging

Packaging:

Part A: 25 kg in a 20-liter iron barrel

Part B: 3 kg in a 5-liter iron barrel.

Shelf Life:

Part A: 12 months    Part B: 12 months

If exceeding shelf life, 

the products shall be tested before using.




H53-5 Epoxy Red Oxide Primer

Applicable Environment


g yj q 5
Chemical plant pipelines

metallurgical equipment

Bridge

Engineering machinery



H53-5 Epoxy Red Oxide Primer

Compatibility



Product Thickness
Primer: H53-2 Epoxy Red Oxide Primer

2*40 µm

Midcoat:

H53-6 Epoxy Mica Iron Oxide Paint

150 µm

Topcoat:

BS52-10 Acrylic Polyurethane Finish Paint

2*40 µm



H53-5 Epoxy Red Oxide Primer

Finished Projects


1 2 3



H53-5 Epoxy Red Oxide Primer

Production Process


4-1 4-2 4-3



H53-5 Epoxy Red Oxide Primer 

Instructions For Use


Substrate Treatment:

All surface shall be clean, dry and free from any contaminations.

       Steel with oxide scale

It should achieve the level of Sa2.5 by sand or shot blasting.

       Steel without oxide scale

It should achieve the level of St3 by mechanical derusting.

Instructions for Use:

Mixing

Mix part A and part B as 25:3 by weight. Slowly add part B into part A and ensure mixed completely.

Thinner

X-7 Epoxy paint thinner ≤ 10 % w./w.

Cleaner

X-7 Epoxy paint thinner

Application methods:

Airless  spray  (recommended):  Nozzle  tip:  0.031-0.041  inch,  pump:  45:1,

pressure: 3600 psi minimum.

Brush: Nylon / Polyester natural bristle.

Roller: 3/8’’ – 1/2’’ woven with solvent resistant core.



H53-5 Epoxy Red Oxide Primer

Company Introduction


8-1
6-1 6-2 6-3 6-4



H53-5 Epoxy Red Oxide Primer

Exhibitions


7-1 7-2 7-3
7-4 7-5 7-6








Previous: 
Next: 
Apply Our Best Quotation
Apply Our Best Quotation
If you have any questions about our products, reach out to YMS Paint customer service team.
    inquiry@jsbj88.com
   +86-18015818726
  +86-519-85506198

Products

Application

Quick Links

© COPYRIGHT 2024 CHANGZHOU YMS NEW MATERIALS TECHNOLOGY CO., LTD. ALL RIGHTS RESERVED.