Use the power mixer to mix the main paint evenly, and then as you stir it, you add the hardener until you get to mix well. Generally, if the temperature is below 10℃, it needs 30 min induction time; If the temperature is over 10℃, it needs 15 min induction time.
Part A: Part B= 20:5 (by weight)
0.27m²/Kg (2mm dry film thickness)
| Availability: | |
|---|---|
Epoxy Acid-resistant Cement
This product is composed of modified epoxy acid-resistant resin, pigment, drier, acid-resistant filler, organic solvent, etc.It has the following resistance characteristics:
|
|
|
|
|
|
Color | Iron oxide red, gray, black, etc. |
Gloss | No gloss, semi-gloss |
Density | ~1.5Kg/L (after mixing) |
Hardness | Epoxy acid-resistant cement curing agent |
Solid Volume | (80±2 )% |
Standard Film thickness | 2mm dry film thickness (about 2500um wet film thickness) |
Theoretical spreading rate | 0.27m²/Kg (2mm dry film thickness) |
Full Cure | (23±2℃) 7d |
Flash Point | 27℃ |
![]() | Epoxy Acid-resistant Cement Product PackagingPackaging: Part A 20kg in a 20-liter iron bucket. Part B 5kg in a 6-liter iron bucket. Shelf Life: 12 months If exceeding shelf life, the products shall be tested before using. |
![]() | ![]() | ![]() | ![]() |
Electroplating Workshop | Sedimentation Tank | Sewage Pipeline | Desulfurization Tower |
| Product | Thickness | |
Primer: | Epoxy Acid-resistant Sealing Primer | 30 µm (dry film thickness) |
Paint: | Epoxy Acid-resistant Cement | 2mm (dry film thickness) |
Topcoat: | Acid-resistant Finish | 2*100 µm (dry film thickness) |
![]() | ![]() | ![]() |
![]() | ![]() | ![]() |
Substrate Treatment:
Before using it on the cement base, the substrate shall be cleaned and without dust and oil. The particles, edges and loose parts of the base floor shall be removed to keep the appearance flat. After the surface treatment, apply one coat of epoxy varnish. Besides, the pits and unevenness shall be repaired with epoxy cement.
Instructions for Use:
Mixing:
Use the power mixer to mix the main paint evenly, and then as you stir it, you add the hardener until you get to mix well. Generally speaking, if the temperature is below 10 ℃, it needs 30 min induction time; if the temperature is over 10℃, it needs 15 min induction time.
Mixing Ratio
Part A: Part B = 20:5 (by weight)
Thinner:
Epoxy paint thinner
Scraping:
Must reach the required dry film thickness
![]() | |||
![]() | ![]() | ![]() | ![]() |
![]() | ![]() | ![]() |
![]() | ![]() | ![]() |
Epoxy Acid-resistant Cement
This product is composed of modified epoxy acid-resistant resin, pigment, drier, acid-resistant filler, organic solvent, etc.It has the following resistance characteristics:
|
|
|
|
|
|
Color | Iron oxide red, gray, black, etc. |
Gloss | No gloss, semi-gloss |
Density | ~1.5Kg/L (after mixing) |
Hardness | Epoxy acid-resistant cement curing agent |
Solid Volume | (80±2 )% |
Standard Film thickness | 2mm dry film thickness (about 2500um wet film thickness) |
Theoretical spreading rate | 0.27m²/Kg (2mm dry film thickness) |
Full Cure | (23±2℃) 7d |
Flash Point | 27℃ |
![]() | Epoxy Acid-resistant Cement Product PackagingPackaging: Part A 20kg in a 20-liter iron bucket. Part B 5kg in a 6-liter iron bucket. Shelf Life: 12 months If exceeding shelf life, the products shall be tested before using. |
![]() | ![]() | ![]() | ![]() |
Electroplating Workshop | Sedimentation Tank | Sewage Pipeline | Desulfurization Tower |
| Product | Thickness | |
Primer: | Epoxy Acid-resistant Sealing Primer | 30 µm (dry film thickness) |
Paint: | Epoxy Acid-resistant Cement | 2mm (dry film thickness) |
Topcoat: | Acid-resistant Finish | 2*100 µm (dry film thickness) |
![]() | ![]() | ![]() |
![]() | ![]() | ![]() |
Substrate Treatment:
Before using it on the cement base, the substrate shall be cleaned and without dust and oil. The particles, edges and loose parts of the base floor shall be removed to keep the appearance flat. After the surface treatment, apply one coat of epoxy varnish. Besides, the pits and unevenness shall be repaired with epoxy cement.
Instructions for Use:
Mixing:
Use the power mixer to mix the main paint evenly, and then as you stir it, you add the hardener until you get to mix well. Generally speaking, if the temperature is below 10 ℃, it needs 30 min induction time; if the temperature is over 10℃, it needs 15 min induction time.
Mixing Ratio
Part A: Part B = 20:5 (by weight)
Thinner:
Epoxy paint thinner
Scraping:
Must reach the required dry film thickness
![]() | |||
![]() | ![]() | ![]() | ![]() |
![]() | ![]() | ![]() |
![]() | ![]() | ![]() |